Vypet VNT 245 is a 45% fiberglass reinforced modified PBT / PET polyester injection molding compound designed for electrical and automotive applications requiring low warp and improved surface finish. Features: High temperature performance; Excellent strength and stiffness; Excellent dimensional stability Typical Applications: Automotive parts; Electric motor housings Information provided by Bieglo Gmbh for Lavergne Performance Compounds |