MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Indorama Auriga Polymers Polyclear™ Perserve 2201 PET Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: Polyclear® Preserve PET 2201 is designed to offer exceptional performance in hot-fill and pasteurized container applications. It has a nominal intrinsic viscosity of 0.82 dl/g. Packaging made from Polyclear® Preserve PET 2201 has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container, even after post-fill heat treatment. Polyclear® Preserve PET 2201 is used successfully in heat-set hot-fill bottles for juice, teas, sports drinks, and foods. Polyclear® Preserve PET 2201 is also used successfully in pasteurized bottles for beer, flavored alcoholic beverages, and other carbonated beverages. This polymer complies with the Federal Food, Drug, and Cosmetic Act for certain food contact applications. Containers made from Auriga Polymers Inc. PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is becoming the packaging material of choice.

Key Words: Excellent clarity and dimensional stability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.801 g/cc>= 0.0289 lb/in³
Density >= 1.39 g/cc>= 0.0502 lb/in³Pycnometer
Particle Mesh Size 28 Mesh28 Mesh0.05% through; Gravimetric determination as manufactured
Viscosity Measurement 0.80 - 0.840.80 - 0.84Intrinsic; 1% Solution in Dichloroacetic Acid
Crystallinity >= 50 %>= 50 %Pycnometer
 
Chemical PropertiesMetricEnglishComments
Acetaldehyde <= 2.00 ppm<= 2.00 ppmGas Chromatography
Diethylene Glycol <= 1.8 %<= 1.8 %Gas Chromatography
Carboxyl End Groups <= 45 meq/kg<= 45 meq/kgTitration
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 252 °C<= 486 °FDSC
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %Karl Fisher Titration as manufactured
 
Descriptive Properties
Chip Size< 2.2 grams/100 chips
ProcessBlow Molding
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indorama Auriga Polymers Polyclear™ Splash 3301 PET Resin
Indorama Auriga Polymers Polyclear™ Refresh 1101 PET Resin
Indorama Auriga Polymers Invista™ Polyclear™ Crystal™ 3302 PET Resin
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester
Dow LIGHTER™ C98 Polyethylene Terephthalate (PET) Resin

PINDOB906 / 126380

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.