MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ashley Polymers Ashlene® D930H Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. Also UV and heat stabilized, available in natural and precolored. Any color other than natural may cause a slight change of properties.

Data provided by the manufacturer

Key Words: Polyamide 12; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Water Absorption 0.20 %24 hrs; ASTM D570
Water Absorption at Saturation 1.1 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 46.0 MPaASTM D638
Elongation at Break 260 %ASTM D638
Flexural Modulus 0.380 GPaASTM D790
Izod Impact, Notched 2.51 J/cmASTM D256
 0.210 J/cm
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 184 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 130 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AdvanSix Aegis® PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6
Ashley Polymers Ashlene® LT940H Nylon 11
Celanese Hytrel® 7246 TPC-ET
EMS-Grivory Grilamid® L 20 HL black 9563 PA12
Covestro MONDUR® TD-65 Polyurethane

PNAB82 / 54507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.