MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:
Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processability, colorable

Applications: fully painted and selectively decorated automotive bumper fascias, molded-color exterior components

Description: Hifax CA186 medium melt flow, reactor grade thermoplastic elastomeric olefin resin has an ecellent balance of impact, stiffnss and apintability. It is based on material produced from Montell's proprietary Catalloy process and was designed primarily for painted automotive bumper fascias that require high durability.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccISO 1183
Linear Mold Shrinkage 0.012 cm/cmTool, Montell
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ISO 868
Tensile Strength, Ultimate 16.0 MPaISO R527-1
Tensile Strength, Yield 15.0 MPaISO R527-1
Elongation at Break >= 500 %ISO R527-1
Elongation at Yield 15 %ISO R527-1
Flexural Modulus 0.610 GPaISO 178
Izod Impact, Notched 0.800 J/cm
@Temperature -40.0 °C
ISO 180
Impact Test 22.0 J
@Temperature -30.0 °C
MAII, E at Max Load, Ductile; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature -30.0 - 100 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °CISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adflex™ Q 200 F Polyolefin
LyondellBasell Adflex™ KS-084P TPO Resin
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer
LyondellBasell Astryn EPF30U Polypropylene Copolymer
Dow INSPIRE™ TF1302 TPO

PMO438 / 53635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.