MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Adflex™ KS-084P TPO Resin
Categories: Polymer; Thermoplastic

Material Notes: Primary Processing Method: Extrusion

Key Features: high melt flow, low modulus, impact resistant thermoplastic olefin, resin, good heat sealability, outstanding puncture resistance, excellent balance of flexibility, excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable

Applications: extrusion coatings on a variety of substrates, film, fiber

Meets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600.

Description: Adflex KS-084P high melt flow, low modulus thermoplastic olefin resin is designed for many commercial and industrial extrusion applications. It is based on material produced from Montell's proprietary Catalloy process. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792B
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444ASTM D2240
Tensile Strength, Yield 6.00 MPa870 psiASTM D638
Elongation at Break 670 %670 %ASTM D638
Elongation at Yield 23 %23 %ASTM D638
Flexural Modulus, 1% Secant 110 MPa16000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched NBNBASTM D256A
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adflex™ KS-021P TPO Resin
LyondellBasell Adflex™ Q 100 F Polyolefin
LyondellBasell Adflex™ Q 200 F Polyolefin
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin
Morgan Advanced Ceramics Sillimantin KS Alumina Silicate

PMO294 / 53587

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.