MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Sarlink® TPV 24555 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24555 is a high performance thermoplastic vulcanizate used in automotive and industrial applications. This product is a medium hardness, low density, UV stabilized grade designed for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Low Density; Low Specific Gravity; Lubricated; Medium Flow; Medium Hardness; UV Stabilized; Weather Resistant

Uses: Expansion Joint; Gaskets; Glazing; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240
 55
@Time 5.00 sec
55
@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 4.34 MPa630 psiFlow; ASTM D412
 4.62 MPa670 psiAcross Flow; ASTM D412
 4.76 MPa
@Treatment Temp. 135 °C,
Time 86400 sec
690 psi
@Treatment Temp. 275 °F,
Time 24.0 hour
Across Flow, Change in Air; ASTM D573
 5.64 MPa
@Treatment Temp. 22.8 °C,
Time 252000 sec
817 psi
@Treatment Temp. 73.0 °F,
Time 70.0 hour
Across Flow, Change in IRM 903 Oil; ASTM D471
Elongation at Break 270 %270 %Flow; ASTM D412
 320 %320 %Across Flow; ASTM D412
 342 %
@Treatment Temp. 135 °C,
Time 86400 sec
342 %
@Treatment Temp. 275 °F,
Time 24.0 hour
Across Flow, Change in Air; ASTM D573
 422 %
@Treatment Temp. 22.8 °C,
Time 252000 sec
422 %
@Treatment Temp. 73.0 °F,
Time 70.0 hour
Across Flow, Change in IRM 903 Oil; ASTM D471
Tear Strength 15.8 kN/m90.0 pliASTM D624
Compression Set 29 %
@Temperature 100 °C,
Time 79200 sec
29 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FInjection, Melt
Rear Barrel Temperature 173 - 213 °C344 - 416 °FInjection
Middle Barrel Temperature 179 - 219 °C354 - 426 °FInjection
Front Barrel Temperature 184 - 224 °C364 - 436 °FInjection
Nozzle Temperature 190 - 230 °C374 - 446 °FInjection
Zone 1 166 - 204 °C330 - 400 °FExtrusion
Zone 2 171 - 210 °C340 - 410 °FExtrusion
Zone 3 177 - 216 °C350 - 420 °FExtrusion
Zone 4 179 - 218 °C355 - 425 °FExtrusion
Zone 5 182 - 221 °C360 - 430 °FExtrusion
Die Temperature 190 - 227 °C374 - 440 °FExtrusion
Mold Temperature 35.0 - 60.0 °C95.0 - 140 °FInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1191 / 237682

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.