MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 24555 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24555 is a high performance thermoplastic vulcanizate used in automotive and industrial applications. This product is a medium hardness, low density, UV stabilized grade designed for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Low Density; Low Specific Gravity; Lubricated; Medium Flow; Medium Hardness; UV Stabilized; Weather Resistant

Uses: Expansion Joint; Gaskets; Glazing; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D2240
 55
@Time 5.00 sec
ASTM D2240
Tensile Strength at Break 630 psiFlow; ASTM D412
 670 psiAcross Flow; ASTM D412
 690 psi
@Treatment Temp. 135 °C,
Time 86400 sec
Across Flow, Change in Air; ASTM D573
 817 psi
@Treatment Temp. 22.8 °C,
Time 252000 sec
Across Flow, Change in IRM 903 Oil; ASTM D471
Elongation at Break 270 %Flow; ASTM D412
 320 %Across Flow; ASTM D412
 342 %
@Treatment Temp. 135 °C,
Time 86400 sec
Across Flow, Change in Air; ASTM D573
 422 %
@Treatment Temp. 22.8 °C,
Time 252000 sec
Across Flow, Change in IRM 903 Oil; ASTM D471
Tear Strength 90.0 pliASTM D624
Compression Set 29 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 374 - 446 °FInjection, Melt
Rear Barrel Temperature 344 - 416 °FInjection
Middle Barrel Temperature 354 - 426 °FInjection
Front Barrel Temperature 364 - 436 °FInjection
Nozzle Temperature 374 - 446 °FInjection
Zone 1 330 - 400 °FExtrusion
Zone 2 340 - 410 °FExtrusion
Zone 3 350 - 420 °FExtrusion
Zone 4 355 - 425 °FExtrusion
Zone 5 360 - 430 °FExtrusion
Die Temperature 374 - 440 °FExtrusion
Mold Temperature 95.0 - 140 °FInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 120 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1191 / 237682

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.