MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Bumpon™ SJ6008 Resilient Rollstock
Categories: Polymer; Adhesive

Material Notes: 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Thickness 3180 microns125 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore M 7272Polyurethane
Tensile Strength at Break 4.14 MPa600 psiDie A; ASTM D412
Elongation at Break 100 %100 %Die A; ASTM D412
Coefficient of Friction, Dynamic >= 1.0>= 1.0Stainless Steel
 >= 1.0>= 1.0Glass
 0.90 - 1.40.90 - 1.4Formica laminate
 0.90 - 1.40.90 - 1.4Wood
Peel Strength 0.526 kN/m3.00 pli90°, Adhesion to Polypropylene
 1.93 kN/m11.0 pli90°, Adhesion to Polystyrene
 4.38 kN/m25.0 pli90°, Adhesion to ABS
 4.38 kN/m25.0 pli90°, Adhesion to Stainless Steel
 4.38 kN/m25.0 pli90°, Adhesion to Aluminum
Taber Abrasion, mg/1000 Cycles 1.7 - 1.91.7 - 1.9H18, 1 kg; ASTM C501
Compression Set 3.0 %3.0 %ASTM D1056
 4.0 %4.0 %25% deflection; ASTM D1056
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 7.87 kV/mm200 kV/inASTM D1000
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °F
 107 °C225 °FIntermittent Exposure
Minimum Service Temperature, Air -34.0 °C-29.2 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 5.00 °C>= 41.0 °FApplication
 <= 52.0 °C<= 126 °FApplication
 
Descriptive Properties
Adhesive TypeA-20 (acrylic)
AppearanceBlack Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35226 / 169973

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.