Description: EUROPLEX® PPSU is a sheet material based on an engineering plastic with further improved fire behavior as compared with the EUROPLEX® F series. Owing to its special properties, EUROPLEX® PPSU also meets the stringent requirements of the OSU heat release test and is therefore suitable for larger items of cabin interiors such as door and door frame panels, monitor housings or oxygen flask holders. Applications: - interior door frames
- wall covers
- monitor housing
Information provided by degussa. Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale. |