MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vyncolit TX10916 Graphite Filled Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.

Information provided by Sumitomo Bakelite North America, Inc.

Key Words: PF-CD65
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.900 g/ccISO 60
Density 1.63 g/ccISO 1183
Water Absorption 0.060 %ISO 62
Linear Mold Shrinkage 0.0044 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPaISO 527-1
Elongation at Break 0.47 %ISO 527-1
Tensile Modulus 19.0 GPaISO 527-1
Flexural Strength 93.0 MPaISO 178
Flexural Modulus 15.0 GPaISO 178
Compressive Strength 162 MPaISO 604
Charpy Impact Unnotched 2.90 kJ/m²ISO 179-1
Charpy Impact, Notched 1.30 kJ/m²ISO 179-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CTMA
CTE, linear, Transverse to Flow 28.0 µm/m-°CTMA
Deflection Temperature at 1.8 MPa (264 psi) >= 166 °CISO 75 Af
Shrinkage 0.080 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
Vyncolit X659 Glass, Mineral and Graphite Filled Novolac Phenolic

PVYNC955 / 142730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.