MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Carbon Fiber Composite

Material Notes: Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 - 0.700 g/cc0.0217 - 0.0253 lb/in³Powder Density; ISO 60
Density 1.35 g/cc0.0488 lb/in³Relative Density; ISO 1183
Water Absorption 0.050 - 0.10 %0.050 - 0.10 %
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm0.00 - 0.0020 in/inInjection Molding; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 - 130 MPa14500 - 18900 psiISO 527
Elongation at Break 0.40 - 0.70 %0.40 - 0.70 %Tensile; ISO 527
Tensile Modulus 20.0 - 23.0 GPa2900 - 3340 ksiISO 527
Flexural Strength 250 - 300 MPa36300 - 43500 psiAt Rupture; ISO 178
Flexural Modulus 17.0 - 24.0 GPa2470 - 3480 ksiISO 178
Flexural Strain at Break 1.2 - 1.5 %1.2 - 1.5 %ISO 178
Compressive Strength 270 - 330 MPa39200 - 47900 psiISO 604
Charpy Impact Unnotched 1.10 - 1.70 J/cm²5.24 - 8.09 ft-lb/in²ISO 179
Charpy Impact, Notched 0.200 - 0.300 J/cm²0.952 - 1.43 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.817e+7 ohm-cm3.817e+7 ohm-cmASTM D257
Surface Resistance 3.669e+6 ohm3.669e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 1.00 - 5.00 µm/m-°C
@Temperature 20.0 °C
0.556 - 2.78 µin/in-°F
@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 25.0 - 40.0 µm/m-°C
@Temperature 20.0 °C
13.9 - 22.2 µin/in-°F
@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 230 - 250 °C446 - 482 °FISO 75 A
Shrinkage 0.00 - 0.10 %0.00 - 0.10 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
Main FillerCarbon Fiber
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Novolac 27%, Carbon fabric 73%
Phenolic 40%, Carbon fabric 60%
Overview of materials for Phenolic, Carbon Fiber Composite
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic

PVYNC067 / 72275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.