MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Self extinguishing (UL-94 V-0) 30% glass fiber reinforced polyamide 6.6 for component with high stiffness and dimensional stability

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³DIN 53479
Water Absorption 6.0 %6.0 %DIN 53495
Moisture Absorption at Equilibrium 1.4 %1.4 %50%RH; DIN 53714
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM-D785
Tensile Strength, Yield 135 MPa19600 psiASTM-D638
Elongation at Break 2.0 %2.0 %ASTM-D638
Flexural Strength 210 MPa30500 psiASTM D790
Flexural Modulus 9.50 GPa1380 ksiASTM-D790
Izod Impact, Notched 1.00 J/cm
@Temperature 23.0 °C
1.87 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN 53482
Surface Resistance 1.00e+12 ohm1.00e+12 ohmDIN 53482
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 70.0 kV/mm1780 kV/inVDE 0303/4
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °F
Maximum Service Temperature, Air 120 °C248 °FContinuous Use
 200 °C392 °FShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FDIN 53461
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade
Polymer Resources PPX-FR3-[color]EN Modified PPO, UL 94 V-1 with HDT of 265 F, Extrusion Grade
Hippe PA 46 Nylon 46
Celanese Celanex® 4202 PBT, 15% Glass Reinforced

PPOLYRA233 / 57495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.