System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Ether/PPO
;
Polyphenylene Ether, Molded
Material Notes:
Process:
Extrusion
Notes:
All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.
Information provided by Polymer Resources Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.08
g/cc
0.0390
lb/in³
ASTM D792
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ASTM D955
Melt Flow
15
-
40
g/10 min
15
-
40
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
56.5
MPa
8200
psi
ASTM D638
Tensile Strength, Yield
46.9
MPa
6800
psi
ASTM D638
Flexural Strength
55.2
MPa
8000
psi
ASTM D790
Flexural Modulus
2.28
GPa
330
ksi
ASTM D790
Izod Impact, Notched
3.74
J/cm
7.00
ft-lb/in
ASTM D256
Gardner Impact
>=
16.9
J
>=
12.5
ft-lb
ASTM D3029
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
87.8
°C
190
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
82.2
°C
180
°F
ASTM D648
Flammability, UL94
V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Processing Properties
Metric
English
Comments
Melt Temperature
246
-
274
°C
475
-
525
°F
Drying Temperature
71.1
-
82.2
°C
160
-
180
°F
Dry Time
3
-
4
hour
3
-
4
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Polymer Resources PPX-FR3-[color]EN Modified PPO, UL 94 V-1 with HDT of 265 F, Extrusion Grade
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade
Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
PPOLYR142 / 57304
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.