MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics Duralan II™ AR Polycarbonate Unshielded Window
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability to laminate together multiple substrates allowing for a fully customized design. This process allows for the incorporation of specialty materials for EMI shielding, light control, polarization and other value added features. The use of polycarbonate or acrylic offers the most flexibility in application design.

Surface Finish Option: Clear anti-reflective or Textured Anti-reflective

Design Options: Screen Printing, Heat Shielding, Privacy Filters and Other Specific Applications Available

Typical Applications: Military, Aerospace, Medical, Industrial, Display Protection and Test Instrumentation

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 180 - 12700 microns
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 74 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
Celanese CoolPoly® E4501 Thermally Conductive Polycarbonate

PCHOME287 / 130997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.