MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Palatinol® 79P Linear Phthalate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Formula: C24H38O4

Description: Palatinol 79P is a predominantly linear phthalate plasticizer based upon C7 and C9 alcohols. The ratio of these alcohols and their degree of linearity provide excellent processing characteristics, superior plastisol rheology and improved product flexibility under low temperature conditions when compared to DOP, DINP and DOTP in PVC resins

Applications: Palatinol 79P is a general purpose phthalate plasticizer and can replace DOP, DOTP and DINP in most applications; it can also replace general purpose blends that contain these plasticizers. Palatinol 79P exhibits better efficiency and imparts lower temperature flexibility than the above mentioned plasticizers. It is particularly useful in plastisol applications because it imparts lower initial viscosity, better viscosity and stability than branched plasticizers. Typical end uses are traffic cones, automotive sealants, fabric coating, fishing lures, extruded profiles and shoe compound.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 - 0.981 g/cc0.0351 - 0.0354 lb/in³ASTM D4052
Solubility of Water 0.0020 %0.0020 %
Solubility in Water <= 1.0e-6 %<= 1.0e-6 %
Viscosity  21 cP
@Temperature 40.0 °C
21 cP
@Temperature 104 °F
Absolute
 46 cP
@Temperature 20.0 °C
46 cP
@Temperature 68.0 °F
Absolute
 162 cP
@Temperature 0.000 °C
162 cP
@Temperature 32.0 °F
Absolute
Molecular Weight 398 g/mol398 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.070<= 0.070[mg KOH/g]; ASTM D1045
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  67
@Time 15.0 sec
67
@Time 0.00417 hour
Plasticizer conc. in vinyl film 70 phr; ASTM D 2240
 79
@Time 15.0 sec
79
@Time 0.00417 hour
Plasticizer conc. in vinyl film 50 phr; ASTM D 2240
 86
@Time 15.0 sec
86
@Time 0.00417 hour
Plasticizer conc. in vinyl film 40 phr; ASTM D 2240
Tensile Strength 12.4 MPa1800 psiPlasticizer conc. in vinyl film 70 phr; ASTM D412
 15.9 MPa2310 psiPlasticizer conc. in vinyl film 50 phr; ASTM D412
 17.9 MPa2600 psiPlasticizer conc. in vinyl film 40 phr; ASTM D412
Elongation at Break 300 %300 %Plasticizer conc. in vinyl film 40 phr; ASTM D412
 350 %350 %Plasticizer conc. in vinyl film 50 phr; ASTM D412
 350 %350 %Plasticizer conc. in vinyl film 70 phr; ASTM D412
100% Modulus  5.86 MPa
@Strain 100 %
850 psi
@Strain 100 %
Plasticizer conc. in vinyl film 70 phr; ASTM D412
 9.65 MPa
@Strain 100 %
1400 psi
@Strain 100 %
Plasticizer conc. in vinyl film 50 phr; ASTM D412
 12.8 MPa
@Strain 100 %
1850 psi
@Strain 100 %
Plasticizer conc. in vinyl film 40 phr; ASTM D412
Torsional Stiffness 931 MPa
@Temperature -40.0 °C
135000 psi
@Temperature -40.0 °F
Plasticizer conc. in vinyl film 70 phr; ASTM D1043
 
Thermal PropertiesMetricEnglishComments
CTE, linear 750 µm/m-°C417 µin/in-°F
Pour Point >= -50.0 °C>= -58.0 °F
Brittleness Temperature -45.0 °C-49.0 °FPlasticizer conc. in vinyl film 70 phr; ASTM D746
Flash Point 218 °C424 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4831.483
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.10 %0.10 %ASTM E203
 
Descriptive Properties
Color<25APAH, ASTM D1209
CompositionEster content>99.0%, ASTM D3465

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite
Pyrotek S-1 Fabric
Pyrotek H-10B Fabric
Phillips Sumika Marlex® HGX-030-01 Polypropylene Homopolymer, Fiber Grade
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer

PBASG0738 / 132371

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.