MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ EC2216 Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: High Performance, Very flexible bonds

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 80000 cP
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 400 psi
@Temperature 82.0 °C
Overlap
 3000 psi
@Temperature -55.0 °C
Overlap
 3200 psi
@Temperature 24.0 °C
Overlap
Peel Strength 25.0 pliT-Peel
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 hourTime to Handling Strength

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M Scotch-Weld™ 2216 B/A Gray Two-Part Epoxy Adhesive 2216 B/A Gray
Aptek DIS-A-PASTE 2310-PMF Thermally conductive adhesive/encapsulant
Piezo Kinetics PKI 556 Lead Zirconate Titanate Piezoelectric
Piezo Kinetics PKI 552 Lead Zirconate Titanate Piezoelectric

PMM34652 / 169399

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.