MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C)

Key Words: Coatings
Vendors: Aremco’s high temperature coatings and sealers are formulated using ceramic, glass and silicone technologies for a broad range of electrical insulation applications. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/cc
Solids Content 43.3 %43.3 %by volume
 55.8 %55.8 %by weight
Volatile Organic Compounds (VOC) Content 104.2 g/l104.2 g/l
Viscosity 50 - 100 cP50 - 100 cP
Thickness 25.4 microns1.00 milrecommended dry film thickness
 58.7 microns2.31 milestimated wet film thickness
Storage Temperature 12.8 - 29.4 °C55.0 - 85.0 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength <= 29.5 kV/mm<= 750 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 482 °C900 °FContinuous
Flash Point >= 100 °C>= 212 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 48.9 °C50.0 - 120 °FApplication Temperature
Cure Time >= 6.00 min>= 0.100 hourAir Set prior to curing
 45.0 min
@Temperature 232 °C
0.750 hour
@Temperature 450 °F
Adequate ventilation required. Outgasses between 300°F and 750°F. Additional 30 minutes is required depending on service temperature.
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorTranslucent-White
Dry Film Coverage ft2/gal695at 1 mil
ThinnerButyl Cellosolve/Water

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay BR® 680-3 Polyimide Film Adhesive
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone

ZPAREM40 / 24304

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.