MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 7828 Thermal Transfer Polyester Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Thermal Transfer Polyester Label Materials are thin profile, gloss polyester label stocks that offer excellent durability and moisture resistance. These label materials utilize 3M™ Adhesive 400 which is designed to offer good peel strength to a variety of surfaces, as well as, excellent clarity and UV resistance.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 20.3 microns0.800 milAdhesive
 25.4 microns1.00 milFacestock
 81.3 microns3.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.05478 kN/m0.3125 pliStainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.07669 kN/m0.4375 pliStainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.0877 kN/m0.500 pliLD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.09861 kN/m0.5625 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.110 kN/m0.625 pliStainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.1205 kN/m0.6875 pliLD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.131 kN/m0.750 pliHD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.131 kN/m0.750 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.153 kN/m0.875 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.153 kN/m0.875 pliStainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.1643 kN/m0.9375 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.1643 kN/m0.9375 pliHD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.18626 kN/m1.0625 pliStainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.18626 kN/m1.0625 pliLD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.18626 kN/m1.0625 pliLD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.20817 kN/m1.1875 pliGlass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.23008 kN/m1.3125 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.23008 kN/m1.3125 pliGlass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.25199 kN/m1.4375 pliStainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.263 kN/m1.50 pliHD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.27391 kN/m1.5625 pliGlass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.2849 kN/m1.625 pliPolypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.2849 kN/m1.625 pliGlass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.29582 kN/m1.6875 pliPolypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.29582 kN/m1.6875 pliPolypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.307 kN/m1.75 pliPolypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.307 kN/m1.75 pliGlass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.31773 kN/m1.8125 pliStainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.31773 kN/m1.8125 pliGlass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.351 kN/m2.00 pliGlass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.351 kN/m2.00 pliPolycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.351 kN/m2.00 pliGlass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.36156 kN/m2.0625 pliPolycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 0.36156 kN/m2.0625 pliPolycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.36156 kN/m2.0625 pliPolypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.3725 kN/m2.125 pliPolypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.40538 kN/m2.3125 pliPolypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.4163 kN/m2.375 pliPolycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.4163 kN/m2.375 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.42729 kN/m2.4375 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.438 kN/m2.50 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.438 kN/m2.50 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.44921 kN/m2.5625 pliPolycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.5040 kN/m2.875 pliPolycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.51494 kN/m2.9375 pliHD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.5478 kN/m3.125 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.73407 kN/m4.1875 pliPolycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= -12.0 °C>= 10.4 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type400 Acrylic
Liner55# Densified Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 7222/7865 Thermal Transfer Polyester Label Material
3M 7816 Thermal Transfer Polyester Label Materials
3M 7813 Thermal Transfer Polyester Label Material
3M 7810 Thermal Transfer Polyester Label Material
3M 7350FL Thermal Transfer Polyester Label Material

PMM33541 / 168288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.