MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
NovaCentrix Metalon® ICI-003 Nanocopper Ink – Aqueous dispersion
Categories: Fluid; Other Engineering Material

Material Notes: ICI-003 is an aqueous, copper oxide-based ink which is transformed post-printing into a metallic copper thin film after it is processed with PulseForge® tools. It is designed to produce very flexible, conductive traces on porous, low-temperature substrates such as Novele™ (a coated PET). ICI-003 is specially formulated for compatibility and stability with piezoelectric inkjet printing methods.

Metalon ICI-003 produces, after printing and curing, conductive, metallic copper traces with electrical resistivities as low as 2.5× bulk Cu resistivity. ICI-003 MUST be processed with PulseForge® tools from NovaCentrix® to attain the stated resistivity values. Thermal curing is not applicable. Printed traces of ICI-003 are not conductive prior to processing with PulseForge® tools.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Particle Size 85 - 115 µmz-avg by DLS
Viscosity 1.0 - 6.5 cP
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000043 ohm-cmExample; on coated PET substrate
Surface Resistivity per Square 0.14 ohmExample; on coated PET substrate
 
Descriptive Properties
CuO Content (wt%)10
Flash pointNon-flammable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2020624D2 Silver Carbon Ink
SunChemical Gwent C2020522D1 Silver Ink
NovaCentrix PSI-219® Conductive Screen Ink
NovaCentrix PSI-211® Conductive Screen Ink
NovaCentrix Metalon® JS-B40G Nanosilver Ink – Aqueous dispersion for Dimatix Printheads

ENOVA904 / 191514

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.