MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2020522D1 Silver Ink  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: C2020522D1 is a screen printable, conductive Silver Ink, designed for applications on Polyester and ITO-coated Polyester Films. This is an easy processing paste, consisting of finely divided silver and carbon particles dispersed in a thermoplastic resin system. This ink is compatible with C2020522D1 Silver Carbon Ink, which can be used in areas where sheet resistivity is not critical.

The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.60 g/cc0.0939 lb/in³
Solids Content 68 - 79 %68 - 79 %
Viscosity 18000 - 20000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
18000 - 20000 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 standard Medium cone (PK1.1°)
Thickness 25.0 microns0.984 mil
Storage Temperature <= 25.0 °C<= 77.0 °Fcool dry place
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000023 ohm-cm0.000023 ohm-cmcured film
Surface Resistivity per Square 0.0145 ohm0.0145 ohmcured film; 25 microns thick
 
Processing PropertiesMetricEnglishComments
Processing Temperature 120 °C248 °F
Dry Time 0.100 hour0.100 hourbelt drier with good air flow
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Abrasion Resistance - Pencil Hardness3HTested on Polyester substrates
AdhesionPencil Hardness Tested on Polyester substrates 3H
Conductive Filler TypeSilver (Ag)
Coverage cm2/g180
Material TypeReady-To-Use Formulation
Printing Mesh counts/inch180 to 340stainless steel or polyester screens
Recommended SubstratesPolyester or ITO coated Polyester
Solvent SystemEthoxy Propanol or Sericol

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NovaCentrix Metalon® JS-A101 Nanosilver Ink – Aqueous dispersions for Inkjet Printing
SunChemical Gwent C2020624D2 Silver Carbon Ink
NovaCentrix PSI-219® Conductive Screen Ink
NovaCentrix PSI-211® Conductive Screen Ink
NovaCentrix Metalon® JS-B40G Nanosilver Ink – Aqueous dispersion for Dimatix Printheads

WGEM031 / 75884

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.