MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Cyclo Olefin Polymer
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 - 1.12 g/ccAverage value: 1.02 g/cc Grade Count:51
Water Absorption 0.0100 - 0.400 %Average value: 0.0342 % Grade Count:24
Water Absorption at Saturation 0.0100 %Average value: 0.0100 % Grade Count:15
Moisture Vapor Transmission 0.0780 - 0.380 cc-mm/m²-24hr-atmAverage value: 0.134 cc-mm/m²-24hr-atm Grade Count:10
Water Vapor Transmission 0.000130 - 3.88 g/m²/day
@Temperature 38.0 - 38.0 °C
Average value: 1.29 g/m²/day Grade Count:3
Thickness 70.0 - 127 micronsAverage value: 82.4 microns Grade Count:7
Linear Mold Shrinkage 0.00100 - 0.00700 cm/cmAverage value: 0.00546 cm/cm Grade Count:12
Melt Flow 0.100 - 130 g/10 minAverage value: 17.3 g/10 min Grade Count:46
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120 - 125Average value: 123 Grade Count:3
Tensile Strength, Ultimate 36.0 - 77.0 MPaAverage value: 56.0 MPa Grade Count:27
Tensile Strength, Yield 46.0 - 63.0 MPaAverage value: 57.2 MPa Grade Count:12
Film Elongation at Break, MD 1.40 - 800 %Average value: 162 % Grade Count:8
Film Elongation at Break, TD 1.10 - 790 %Average value: 159 % Grade Count:8
Elongation at Break 1.50 - 140 %Average value: 36.4 % Grade Count:34
Elongation at Yield 1.70 - 4.50 %Average value: 2.84 % Grade Count:7
Modulus of Elasticity 1.25 - 5.49 GPaAverage value: 2.39 GPa Grade Count:37
Flexural Yield Strength 55.0 - 130 MPaAverage value: 98.4 MPa Grade Count:14
Flexural Modulus 1.60 - 5.17 GPaAverage value: 2.48 GPa Grade Count:33
 1.70 - 2.70 GPa
@Temperature 40.0 - 130 °C
Average value: 2.13 GPa Grade Count:2
Izod Impact, Notched 0.100 - 30.0 J/cmAverage value: 1.56 J/cm Grade Count:28
Izod Impact, Unnotched (ISO) 10.0 - 33.0 kJ/m²Average value: 17.2 kJ/m² Grade Count:6
Charpy Impact Unnotched 1.30 - 2.00 J/cm²Average value: 1.56 J/cm² Grade Count:8
Charpy Impact, Notched 0.160 - 3.60 J/cm²Average value: 0.570 J/cm² Grade Count:9
Elmendorf Tear Strength MD 9.00 - 2720 gAverage value: 647 g Grade Count:6
Elmendorf Tear Strength TD 9.00 - 3170 gAverage value: 732 g Grade Count:6
Dart Drop Test 36.0 gAverage value: 36.0 g Grade Count:5
Film Tensile Strength at Break, MD 35.0 - 60.7 MPaAverage value: 53.9 MPa Grade Count:8
Film Tensile Strength at Break, TD 25.0 - 57.0 MPaAverage value: 48.7 MPa Grade Count:8
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmAverage value: 1.00e+16 ohm-cm Grade Count:12
Dielectric Constant 2.20 - 3.00Average value: 2.36 Grade Count:21
Dielectric Strength 30.0 - 157 kV/mmAverage value: 62.5 kV/mm Grade Count:7
Dissipation Factor 0.0000700 - 0.0200Average value: 0.00287 Grade Count:17
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:6
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 80.0 µm/m-°CAverage value: 67.8 µm/m-°C Grade Count:23
Thermal Conductivity 0.170 - 0.180 W/m-K
@Temperature 100 - 100 °C
Average value: 0.175 W/m-K Grade Count:2
Melting Point 80.0 - 155 °CAverage value: 120 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 170 °CAverage value: 122 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 162 °CAverage value: 112 °C Grade Count:13
Vicat Softening Point 64.0 - 178 °CAverage value: 123 °C Grade Count:7
Heat Distortion Temperature 105 - 144 °CAverage value: 131 °C Grade Count:4
Glass Transition Temp, Tg 65.0 - 178 °CAverage value: 124 °C Grade Count:47
Flammability, UL94 HB - V-2Grade Count:12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51 - 1.54Average value: 1.53 Grade Count:25
Abbe Number 56.0 - 57.0Average value: 56.7 Grade Count:3
Haze 0.600 - 4.00 %Average value: 1.73 % Grade Count:14
Gloss 94.0 - 116 %Average value: 101 % Grade Count:6
Transmission, Visible 90.0 - 93.0 %Average value: 91.6 % Grade Count:35
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 320 °CAverage value: 268 °C Grade Count:8
Melt Temperature 84.0 - 320 °CAverage value: 251 °C Grade Count:9
Mold Temperature 40.0 - 160 °CAverage value: 100 °C Grade Count:9
Injection Velocity 20.0 - 150 mm/secAverage value: 94.3 mm/sec Grade Count:7
Injection Pressure 40.0 - 120 MPaAverage value: 80.0 MPa Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Low Density Polyethylene (LDPE), Molded
Zeon Specialty Materials ZEONEX® 480 Cyclo Olefin Polymer
Polyplastics TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
Overview of materials for Styrene-Butadiene Copolymer, SBC

O4310 / 77788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.