MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grivory® HT3Z LF black 9564 PA*
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially based on renewable raw materials. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide Grivory HT3Z LF is especially used in tribological applications. Grivory HT3Z LF exhibits low moisture absorption, high stiffness and high heat distortion temperature. The PTFE (polytetrafluoroethylene) modification reduces the sliding friction after a short initial phase. As each tribological system has its own properties (material combination, temperature, force etc.), the suitability of the product has to be tested for each application under practical conditions.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDry; ISO 1183
Water Absorption 2.5 %Sim. to ISO 62
Moisture Absorption 1.40 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 140 MPaDry; ISO 2039-1
 140 MPaConditioned; ISO 2039-1
Tensile Strength at Break 75.0 MPaConditioned; ISO 527-1/-2
 80.0 MPaDry; ISO 527-1/-2
Elongation at Break 3.0 %Dry; ISO 527-1/-2
 4.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 2700 MPaDry; ISO 527-1/-2
 2800 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 33.0 kV/mmDry; IEC 60243-1
 33.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 400 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 295 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °CLong Term; ISO 2578
 240 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 110 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 85.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Cooling and climate control
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsElectrical appliances
 Electrical equipment
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Co Polyamide
 Hydrolysis resistant
 Improved alcohol resistance
 Partially aromatic Polyamide
Special CharacteristicsImproved heat resistance
 Platable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
EMS-Grivory Grilamid® LV-3H PA12-GF30
EMS-Grivory Grilamid® LKN-5H PA12-GB50
EMS-Grivory Grivory® HT3Z black 9564 PA*
Celanese Zytel® 101L NC010 PA66

PGRH392 / 157101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.