MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone with glass fiber, easy flowing, demolding aid
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Properties/attributes include: High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range. Especially suitable for thin wall complex parts. Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistance

Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical engineering, aircraft- and aerospace industry. Typical uses include: High quality terminal bar, switches and plugs, relays, lamp reflectors, sterilizable medical equipment.

Processing: During processing the moisture level should not exceed 0.05%, otherwise porosity and surface defects (e.g. smearing) may occur. To avoid internal stresses, a low shear load should be used for processing. The parts may be tempered at a later stage to reduce internal stresses. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmDIN 16901
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130 MPaISO 527-2
Elongation at Break 2.4 %ISO 527-2
Modulus of Elasticity 8.00 GPaISO 527-2
Flexural Strength 150 MPaISO 178
Flexural Modulus 6.00 GPaISO 178
Flexural Strain at Break 3.8 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 43.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1fu
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cmIEC 60167
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µm/m-°CDIN 53752
Thermal Conductivity 0.330 W/m-KDIN 52612
Maximum Service Temperature, Air 180 °CContinuous; UL 746B
 200 °CShort Term
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-2/A
Vicat Softening Point 220 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 340 - 360 °C
Zone 1 355 - 375 °C
Zone 2 360 - 380 °C
Zone 3 350 - 370 °C
Melt Temperature 350 °C
Mold Temperature 120 - 200 °C
Drying Temperature 150 °C
@Time 10800 - 18000 sec
Dehumidifying dryer
Moisture Content <= 0.050 %
 
Descriptive Properties
Colornatural color (beige)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
Ensinger TECANYL™ MT Autoclavable Polymer
Ensinger Tecaform™ MT Acetal, Medical Grade (POM)
EMS-Grivory Grilamid® TR 90 LXS PAMACM12

PLUU8815 / 193774

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.