MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® TR 90 LXS PAMACM12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing aid to improve the flow- and demoulding properties. Grilamid TR 90 LXS natural offers outstanding properties such as:
  • Transparency
  • Unlimited colorability
  • Stress crack resistance
  • Toughness and stiffness
  • Good chemical resistance
  • High flexural fatigue strength
  • EU and FDA food approval
Grilamid TR 90 LXS natural is especially suited for injection molded outdoor applications in the application fields of:
  • Optics
  • Automotive
  • Mechanical engineering
  • Safety technology
  • Electro / Electronics

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³Dry; ISO 1183
Water Absorption 3.0 %3.0 %Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 85.0 MPa12300 psiConditioned; ISO 2039-1
Tensile Strength at Break 40.0 MPa5800 psiConditioned; ISO 527-1/-2
Tensile Strength, Yield 60.0 MPa8700 psiConditioned; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 1.50 GPa218 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Maximum Service Temperature, Air 80.0 °C176 °FLong Term; ISO 2578
 95.0 °C203 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75-1/-2
Glass Transition Temp, Tg 125 °C257 °F10°C/min; ISO 11357-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
 Mobile phones and other portable devices
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Sanitary, water and gas supply
 Sports & Leisure
 Tools & Accessories
OpticsOptical components
 Safety glasses
 Spectacle frames
 Sunglasses
ProcessingInjection Molding
Product AttributesImproved alcohol resistance
 Improved flowability and demolding
Special CharacteristicsTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 90 PAMACM12
EMS-Grivory Grilamid® TR 90 NZZ nat PAMACM12-I
EMS-Grivory Grilamid® TR 90 TL PAMACM12
EMS-Grivory Grilamid® TR 90 NZ PAMACM12-I
EMS-Grivory Grilamid® TR 90 UV PAMACM12

PGRH102 / 156811

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.