MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nurel Engineering Polymers Promyde® B30 P2 HI PA 6, Conditioned, Impact modified and Heat stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Impact Grade

Material Notes: Characteristics: Promyde B30 P2 HI is a polyamide 6 high impact modified and heat stabilized.

Applications: Promyde B30 P2 HI allows a fast and efficient mould filling, and an easy mould release, that combined with its excellent mechanical and high impact resistant properties, make it suitable for components requiring very high resistance to breakage by impact.

Information provided by Nurel Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption 2.40 %2.40 %50%, rh; ISO 62
Water Absorption at Saturation 7.6 %7.6 %in water; ISO 62
Viscosity Test 125 cm³/g1.25 dl/gViscosity Number; ISO 307
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm0.0070 - 0.010 in/in
Melt Flow 70 g/10 min
@Load 5.00 kg,
Temperature 275 °C
70 g/10 min
@Load 11.0 lb,
Temperature 527 °F
[cm3/10 min], MVR; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 MPa5080 psi50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1/-2
Elongation at Yield 35 %35 %50 mm/min; ISO 527-1/-2
Tensile Modulus 1.10 GPa160 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 20.0 MPa2900 psi2 mm/min; ISO 178
Flexural Modulus 0.400 GPa58.0 ksi2 mm/min; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 12.5 J/cm²
@Temperature 23.0 °C
59.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDSC 10°C/min; ISO 3146
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °Finjection molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature <= 80.0 °C<= 176 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Nurel Engineering Polymers Promyde® B30 P2 HI PA 6, Dry, Impact modified and Heat stabilized
Envalior Akulon® K125/A PA6

PNUREL032 / 183397

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.