MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A single component, low viscosity, UV curable adhesive designed for curing in seconds. It is an all-purpose, general adhesive for optical applications including fiber optic components, DVD, medical, and PCB level electro-optics. It can also be used for sealing and coating applications. It meets the requirements of USP Class VI biocompatibility standards for medical implants.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Viscosity 150 - 250 cP
@Temperature 23.0 °C
150 - 250 cP
@Temperature 73.4 °F
100 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484
Tensile Modulus 1.73 GPa251 ksiStorage
Shear Strength >= 7.03 MPa>= 1020 psiDie
 
Thermal PropertiesMetricEnglishComments
CTE, linear 69.0 µm/m-°C38.3 µin/in-°FBelow Tg
 170 µm/m-°C94.4 µin/in-°FAbove Tg
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 70.0 °C>= 158 °FPost-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Decomposition Temperature 385 °C725 °FDegradation Temperature
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4736
@Wavelength 589 nm
1.4736
@Wavelength 589 nm
Transmission, Visible >= 98 %
@Wavelength 420 - 1600 nm
>= 98 %
@Wavelength 420 - 1600 nm
Spectral
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
ColorClear/Colorlessbefore cure
ConsistencyPourable liquid
Number of ComponentsSingle
Weight Loss0.79%200°C
 1.2%250°C
 1.9%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy
Epoxyset Epoxiohm EO-98HT Electrically Conductive Epoxy Adhesive
Epoxy Technology EPO-TEK® OG198-54 UV Cure Optical Epoxy
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Epoxy, Molded, Glass Fiber Filler

PPOXYT171 / 141210

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.