MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.

Flexirene FG 23 U represents the version of Flexirene FG 20 U with slip and antiblock agents.

Main Applications: Flexirene FG 23 U is recommended for the production of general purpose film, industrial liners and shoppers; its use is suggested both in blend and in coextrusion with LDPE.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.918 g/ccISO 1183
Thickness 15.0 - 50.0 micronsRecommended
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPaISO 527-3
Film Elongation at Break, MD 600 %ISO 527-3
Film Elongation at Break, TD 750 %ISO 527-3
Coefficient of Friction, Dynamic 0.11ISO 8295
Elmendorf Tear Strength, MD 2.5475 g/micronISO 6383-2
Elmendorf Tear Strength, TD 17.323 g/micronISO 6383-2
Dart Drop Test 120 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 42.0 MPaISO 527-3
Film Tensile Strength at Break, TD 33.0 MPaISO 527-3
1% Secant Modulus, MD 150 MPaISO 527-3
1% Secant Modulus, TD 175 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 123 °CInternal method
Vicat Softening Point 101 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 15 %ISO 14782
Gloss 50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 3026F Low Density Polyethylene (LDPE), Blown Film Grade
LyondellBasell Lupolen 3010D Low Density Polyethylene (LDPE), Blow Molding Grade
Versalis Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion
Versalis Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene
Versalis Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion

PENG092 / 124486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.