MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel REX® M2 S High Speed Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: REX M2 is a tungsten-molybdenum high speed steel which gives outstanding performance in all operations where a general purpose high speed steel is required. REX M2 has a wide hardening range, excellent toughness, with good wear and red hardness characteristics. REX M2S is the sulfur-bearing counterpart of REX M2. The sulfur addition provides good grindability and an improvement in machinability of 25 to 35 per cent over a comparable nonsulfurized grade.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217 - 255217 - 255
Hardness, Rockwell C  57
@Tempering Temp. 649 °C
57
@Tempering Temp. 1200 °F
hardened at 2250°F then tempered
 59
@Tempering Temp. 635.0 °C
59
@Tempering Temp. 1175 °F
hardened at 2250°F then tempered
 60.9
@Tempering Temp. 621 °C
60.9
@Tempering Temp. 1150 °F
hardened at 2250°F then tempered
 62.4
@Tempering Temp. 607.2 °C
62.4
@Tempering Temp. 1125 °F
hardened at 2250°F then tempered
 64
@Tempering Temp. 593 °C
64
@Tempering Temp. 1100 °F
hardened at 2250°F then tempered
 65
@Tempering Temp. 579.4 °C
65
@Tempering Temp. 1075 °F
hardened at 2250°F then tempered
 66
@Tempering Temp. 524 °C
66
@Tempering Temp. 975 °F
hardened at 2250°F then tempered
 66
@Tempering Temp. 566 °C
66
@Tempering Temp. 1050 °F
hardened at 2250°F then tempered
 66.8
@Tempering Temp. 538 °C
66.8
@Tempering Temp. 1000 °F
hardened at 2250°F then tempered
 66.8
@Tempering Temp. 551.7 °C
66.8
@Tempering Temp. 1025 °F
hardened at 2250°F then tempered
Modulus of Elasticity 207 GPa30000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 21.1 - 260 °C
6.40 µin/in-°F
@Temperature 70.0 - 500 °F
 11.8 µm/m-°C
@Temperature 21.1 - 427 °C
6.58 µin/in-°F
@Temperature 70.0 - 800 °F
 12.1 µm/m-°C
@Temperature 21.1 - 538 °C
6.72 µin/in-°F
@Temperature 70.0 - 1000 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 832 °C1530 °FCritical Thermal Treatment Temperature
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.85 %0.85 %
Chromium, Cr 4.15 %4.15 %
Iron, Fe >= 81 %>= 81 %as balance
Manganese, Mn 0.30 %0.30 %
Molybdenum, Mo 5.0 %5.0 %
Silicon, Si 0.30 %0.30 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 6.4 %6.4 %
Vanadium, V 1.95 %1.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel PM M2 Tool Steel
Crucible Steel Rex M2 High Speed Steel
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2

NCRUC912 / 160363

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.