MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crucible Steel PM M2 Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine carbides with essentially no carbide segregation. PM M2 tools will have a finer grain size, much better toughness, and superior grindability in the heat treated condition compared to those made from conventional M2. The higher carbon content (1.00% vs. 0.85%) of PM M2 permits higher attainable hardness. It also offers improved hardenability and gives better heat treat response in larger tool sections. PM M2’s other general characteristics and physical properties are similar to conventionally produced M2.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217 - 255217 - 255Annealed
Hardness, Rockwell C 63 - 6563 - 65
Modulus of Elasticity 207 GPa30000 ksi
Charpy Impact 35.0 J25.8 ft-lbAustenitizing Temperature- 1150°C; Tempering Temperature- 580°C
 37.0 J27.3 ft-lbAustenitizing Temperature- 1175°C; Tempering Temperature- 565°C
 41.0 J30.2 ft-lbAustenitizing Temperature- 1190°C; Tempering Temperature- 550°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 - 260 °C
6.39 µin/in-°F
@Temperature 68.0 - 500 °F
 12.1 µm/m-°C
@Temperature 20.0 - 540 °C
6.72 µin/in-°F
@Temperature 68.0 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.0 %1.0 %
Chromium, Cr 4.15 %4.15 %
Iron, Fe 81.5 %81.5 %As Remainder
Molybdenum, Mo 5.0 %5.0 %
Tungsten, W 6.4 %6.4 %
Vanadium, V 1.95 %1.95 %
 
Descriptive Properties
Grindability; Metal Removed/Wheel Worn6.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel Rex M2 High Speed Steel
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
AISI Type A2 Tool Steel
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Crucible Steel AIRKOOL® (AISI A2) Tool Steel

NCRUC006 / 15999

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.