MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear Diamond Class® Turbine Oil 100
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Diamond Class Turbine Oil is an extended service life rust- and oxidation-inhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Diamond Class Turbine Oil is specially formulated with proprietary additive chemistry to meet the demands of severe- and long-life turbine service. Hydroclear Diamond Class Turbine Oil has demonstrated successful performance results in severe duty General Electric Frame 7 gas turbines used in co-generation service, easily surpassing historical performance of “premium” turbine oils. It can also be used successfully in steam turbines and other applications which require premium quality rust- and oxidation-inhibited circulating oils.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.25 lb/gal
Viscosity Measurement 100Viscosity Index
Saybolt Viscosity at 100°F 495 SUS
Saybolt Viscosity at 210°F 63 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt
Oxidative Stability 17500 hourASTM D 943
ASTM Color 0.50
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 30.0 kV/mmNo thickness given; ASTM D877
 
Thermal PropertiesOriginal ValueComments
Pour Point -20.0 °F
Rotating Bomb Oxidation Test (RBOT) 1900 minASTM D 2272
Flash Point 490 °F
 
Descriptive Properties
Corrosion, Copper Strip1AASTM D130
Emulsion Characteristics (40-40-0)10 minutesWater Separation
Foam Control (Sequence I,II,III)0-0-0
ZincMax 10 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary Megolon™ S642 Low Smoke Halogen Free

WCON083 / 75120

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.