MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AlphaGary Megolon™ S642 Low Smoke Halogen Free
Categories: Polymer; Thermoplastic

Material Notes: A thermoplastic, halogen free, fire retardant, low smoke and fume cable compound. This sheathing grade exhibits an excellent level of fire retardancy and has been developed to meet the requirements of CENELEC HD 624 part 7 S1. Application examples include Low and high voltage power cables / Telecommunications cables / Data Cables.

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 12.5 MPa1810 psi
Elongation at Break 150 %150 %IEC60811-1-1
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 143 °C290 °FTemperature Index
Oxygen Index 40 %40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary Megolon™ S540E Low Smoke Halogen Free
AlphaGary Megolon™ S500 Low Smoke Halogen Free
ConocoPhillips Hydroclear Diamond Class® Turbine Oil 100
Celanese VECTRA S540 LCP, 40% Mineral Reinforced
AlphaGary Megolon™ S800 Low Smoke Halogen Free

PGARY9820 / 140606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.