MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Quartzel® Fused Quartz Textiles
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is available in the form of yarn, roving, chopped strands, wool, and felts.

It is used in dielectric applications (radomes, circuit boards), thermal applications (high temp insulation for aerospace, asbestos replacement, furnace linings, hot gas filtration), and reinforcement for composites (with resins such as phenolics or epoxies).

Information provided by Saint-Gobain Quartz PLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 7.0
Tensile Strength, Ultimate 6000 MPaVirgin Filament
Elongation at Break 7.7 %Virgin Filament
Modulus of Elasticity 78.0 GPaVirgin Filament
Poissons Ratio 0.16
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 6.00e+10 ohm-cm
@Temperature 800 °C
Dielectric Constant 3.74
@Frequency 1e+9 Hz
Dielectric Strength 37.0 kV/mm
Dissipation Factor 0.00020
@Frequency 1e+9 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.540 µm/m-°C
@Temperature 20.0 °C
isotropic (axial vs. radial)
Specific Heat Capacity 0.750 J/g-°C
Thermal Conductivity 1.38 W/m-K
Maximum Service Temperature, Air 1050 °C
Softening Point 1700 °C
Annealing Point 1220 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4585
 
Component Elements PropertiesOriginal ValueComments
SiO2 99.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
S-Glass Fiber, Generic
UBE Tyrannohex® Heat Resistant Composite
AGY ZenTron® S-2 Generic S-Glass Fiber
A-Glass Fiber, Generic
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber

CSTGQZ10 / 2228

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.