MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oilite® Bronze Bearing Alloy - SAE 841
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Oilite® self-lubricating bearing products are made by a powder metallurgy process, allowing close control on the manufacturing process. They contain large interconnected pores to channel lubricants to the areas between shaft and bearing. It is used in appliances, business machines, cylinders, exercise equipment, lawn and garden equipment, medical applications, material handling, packaging and printing machines, and tools.

Oilite® is the Registered US Trademark of Beemer Precision, Inc.

Key Words: ASTM B-438-95A GR 1 Type II; MIL-B-5687D Type 1 GR 1; MPIF CT-1000-K26
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.40 - 6.80 g/cc
Porosity >= 18 %(% oil by volume)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 14000 psi
Elongation at Break 1.0 %1 inch
Compressive Yield Strength 11000 psi0.001 inch permanent set on 1.25 inch diameter by 1 inch long test specimen
Limiting Pressure Velocity <= 50000 psi-ft/min
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 1.75 %
Copper, Cu 87.5 - 90.5 %
Iron, Fe <= 1.0 %
Other, total <= 0.50 %
Tin, Sn 9.5 - 10.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Super Oilite® Iron-Copper Bearing Alloy - SAE 863
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper
Super Oilite® 16 Iron-Copper Bearing Alloy
High-leaded brass, 62%, UNS C35300

NOIL100 / 18518

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.