MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, and Sand.

Applications: General-utility bearings and bushings, automobile fittings.

Classified under: High-leaded tin bronzes. ASTM B584; formerly ASTM B144-3B

Typical data for sand-cast test bars. Alloy does not respond to heat treating

Key Words: High lead tin bronze, ASTM B584, ASTM B144-3B, SAE 660
Vendors: Dura-Bar Metal Services is a major distributor of bronze alloys. We stock a large inventory of C93200 in tubes and rounds. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com for more information.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.93 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6565
Tensile Strength, Ultimate 240 MPa34800 psi
Tensile Strength, Yield 125 MPa
@Strain 0.5 %
18100 psi
@Strain 0.5 %
Elongation at Break 20 %20 %in 50 mm
Modulus of Elasticity 100 GPa14500 ksi
Compressive Strength 315 MPa45700 psiat permanent set of 10%
Fatigue Strength 110 MPa
@# of Cycles 1.00e+8
16000 psi
@# of Cycles 1.00e+8
rotating beam
Machinability 70 %70 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 8.00 J5.90 ft-lb
Coefficient of Friction 0.100.10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
0.0000144 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 0.000 - 100 °C
10.0 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 59.0 W/m-K
@Temperature 20.0 °C
409 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 315 °C599 °FIncipient
 855 - 975 °C1570 - 1790 °F
Solidus 855 °C1570 °F
Liquidus 975 °C1790 °F
Shrinkage 1.8 %1.8 %Patternmaker's Shrinkage (7/32 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 260 °C500 °FStress-Relieving Temperature
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb <= 0.35 %<= 0.35 %
Copper, Cu 81 - 85 %81 - 85 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb 6.0 - 8.0 %6.0 - 8.0 %
Nickel, Ni <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.15 %<= 0.15 %
Silicon, Si <= 0.0030 %<= 0.0030 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 6.3 - 7.5 %6.3 - 7.5 %
Zinc, Zn 2.0 - 4.0 %2.0 - 4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Oilite® Bronze Bearing Alloy - SAE 841
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper
MetalTek MTEK 83-7-7-3 Cast UNS C93200 Bearing Bronze
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Sand Cast

MC93200b1 / 11945

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.