MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics WIN-SHIELD™ C (Cast Allycarbonate) EMI Shielded Window
Categories: Polymer

Material Notes: Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast polycarbonate. A unique feature of Parker Chomerics window products is the capability to laminate together multiple substrates allowing for a fully customized design. This process allows for the incorporation of specialty materials for EMI shielding, light control, polarization and other value added features. Polycarbonate is a monolithic product designed for high temperature applications

Surface Finish Option: Clear-Gloss or Medium Non-Glare Finish and Anti-Reflective Surfaces

Design Options: Screen Printing, Heat Shielding, Privacy Filters & Other Specific Designs are Available

Typical Applications: Ruggedized Displays, Military, Aerospace, Industrial Applications, Medical, Test Instruments and EMI Shielding for Touch Screen

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 1500 - 6000 microns59.1 - 236 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness 73 - 105 dB
@Frequency 1e+8 Hz
73 - 105 dB
@Frequency 1e+8 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 63 - 85 %63 - 85 %Mesh Only

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME280 / 130990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.