MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics WIN-SHIELD™ C (Cast Allycarbonate) EMI Shielded Window
Categories: Polymer

Material Notes: Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast polycarbonate. A unique feature of Parker Chomerics window products is the capability to laminate together multiple substrates allowing for a fully customized design. This process allows for the incorporation of specialty materials for EMI shielding, light control, polarization and other value added features. Polycarbonate is a monolithic product designed for high temperature applications

Surface Finish Option: Clear-Gloss or Medium Non-Glare Finish and Anti-Reflective Surfaces

Design Options: Screen Printing, Heat Shielding, Privacy Filters & Other Specific Designs are Available

Typical Applications: Ruggedized Displays, Military, Aerospace, Industrial Applications, Medical, Test Instruments and EMI Shielding for Touch Screen

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1500 - 6000 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 73 - 105 dB
@Frequency 1e+8 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -60.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 63 - 85 %Mesh Only

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME280 / 130990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.