MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ampco Metal AMPCOLOY® 32 Tin leaded Bronze, Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: A general bearings alloy with tin added for higher strength. Resists mild acid. Specific pressure up to 25 MPa. Linear speed up to 10 m/sec.

Applications:

Key Words: CDA 94400; DIN 1716 CuPb10Sn 2.1176.04; DIN 1716 CuPb10Sn 2.1176.03; DIN 1716 CuPb10Sn 2.1176.01; AFNOR U Pb8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070HB 10
Tensile Strength, Ultimate 230 MPa33400 psi
Tensile Strength, Yield 110 MPa
@Strain 0.2 %
16000 psi
@Strain 0.2 %
Elongation at Break 12 %12 %
Modulus of Elasticity 77.0 GPa11200 ksi
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb <= 0.50 %<= 0.50 %
Copper, Cu 78 - 82 %78 - 82 %
Lead, Pb 8.0 - 11 %8.0 - 11 %
Nickel, Ni <= 1.5 %<= 1.5 %
Other, total <= 0.50 %<= 0.50 %
Tin, Sn 9.0 - 11 %9.0 - 11 %
Zinc, Zn <= 2.0 %<= 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 32 Tin leaded Bronze, Castings
Ampco Metal AMPCOLOY® 30 Leaded Bronze, Continuous Cast
Ampco Metal AMPCOLOY® 35 Tin Bronze, Centrifugally Cast
Ampco Metal AMPCOLOY® 35 Tin Bronze, Castings
Ampco Metal AMPCOLOY® 712 Tin Bronze, Continuous Cast

NAMPCO52 / 15006

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.