MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ampco Metal AMPCOLOY® 35 Tin Bronze, Centrifugally Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: Copper Alloy with specific pressure up to 40 MPa and linear speed up to 7 m/sec.

Applications: Axle-bearing and coupling rod bearings, plain bearing for general mechanical engineering applications; Medium stressed bearing pads and adjusting gibs; Normally and highly stressed plain bearing bushing using shafts of unhardened steels; When light edge loading is involved.

Key Words: CDA C 93200; DIN 1705 CuSN7ZnPb 2.1090.04; DIN 1705 CuSN7ZnPb 2.1090.03; DIN 1705 CuSN7ZnPb 2.1090.01; AFNOR U-E 7 Z5 Pb4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7575HB 10
Tensile Strength, Ultimate 240 MPa34800 psi
Tensile Strength, Yield 130 MPa
@Strain 0.2 %
18900 psi
@Strain 0.2 %
Elongation at Break 13 %13 %
Modulus of Elasticity 102 GPa14800 ksi
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb <= 0.30 %<= 0.30 %
Copper, Cu 81 - 85 %81 - 85 %
Lead, Pb 5.0 - 7.0 %5.0 - 7.0 %
Nickel, Ni <= 2.0 %<= 2.0 %
Other, total <= 0.50 %<= 0.50 %
Tin, Sn 6.0 - 8.0 %6.0 - 8.0 %
Zinc, Zn 3.0 - 5.0 %3.0 - 5.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 35 Tin Bronze, Castings
Ampco Metal AMPCOLOY® 35 Tin Bronze, Continuous Cast
Ampco Metal AMPCOLOY® 712 Tin Bronze, Castings
Ampco Metal AMPCOLOY® 712 Tin Bronze, Continuous Cast
Ampco Metal AMPCOLOY® 32 Tin leaded Bronze, Continuous Cast

NAMPCO56 / 15010

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.