MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® 440 Ceramic Fiber Paper
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: 440 paper is a low-cost, high-strength composite paper made from a combination of ceramic fiber, inert fillers, and reinforcing fiberglass. The fiberglass gives added strength to the 440 paper at operating temperatures between 450 and 1300°F. This product is formulated with a fire retardant smoke suppressant reducing the effects of the organic binder burnout.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 13.0 lb/ft³
Loss On Ignition 9.5 %including binder
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 psiAs manufactured
Tensile Strength, Yield 86.0 psiAs manufactured
Compressive Strength 5.00 psi10% deformation
 34.0 psi25% deformation
 489 psi50% deformation
 
Thermal PropertiesOriginal ValueComments
Melting Point 982 °C
Maximum Service Temperature, Air 704 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 32 - 35 %
Fe2O3 <= 2.0 %
SiO2 42 - 46 %
 
Descriptive Properties
ColorGray
Na2O3 (%)<2
Temperature Grade (°C)870

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceraform 100 Ceramic Fiber
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® 110 Ceramic Fiber Paper
Unifrax Fiberfrax® Duraback® Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator

CUNIF001 / 97773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.