MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-ABS 3525 Clear
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Data provided by Multibase.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792-91
Melt Flow 5.0 g/10 min(Condition I) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D785-95
Tensile Strength, Ultimate 31.0 MPaASTM D638-95
Elongation at Break 25 %ASTM D638-95
Flexural Strength 69.0 MPaASTM D790-95
Flexural Modulus 2.414 GPaRT; ASTM D-790-95
Izod Impact, Notched 1.07 J/cmASTM D256-93a
 
Optical PropertiesOriginal ValueComments
Gloss 40 - 70 %ASTM D2457-90
Transmission, Visible 90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accucomp ABS ABS881L Clear Grade
Multibase Multi-ABS 3075 High Impact
Evonik TrogamidĀ® T5000 Nylon 6-3
PTS TristarĀ® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized

PLA298 / 49695

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.