MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-ABS 3075 High Impact
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Data provided by Multibase.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792-91
Melt Flow 5.0 g/10 min5.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785-95
Tensile Strength, Ultimate 37.2 MPa5400 psiASTM D638-95
Elongation at Break 25 %25 %ASTM D638-95
Flexural Strength 53.8 MPa7800 psiASTM D790-95
Flexural Modulus 2.00 GPa290 ksiRT; ASTM D-790-95
Izod Impact, Notched 4.00 J/cm7.49 ft-lb/inASTM D256-93a
Gardner Impact 10.6 J7.82 ft-lbASTM D5420-93
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.4 kV/mm899 kV/inASTM D149-95
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 212 °C414 °Finjection molded annealed; ASTM D-648-95
Vicat Softening Point 107 °C225 °FASTM D1525-95
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Multibase Multi-ABS 3525 Clear
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Polymer Resources PPX-FR3-[color]EN Modified PPO, UL 94 V-1 with HDT of 265 F, Extrusion Grade
ITW Spraycore® SC 4000 HDT Mold Building Compound

PLA291 / 49688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.