MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zell-Metall Engineering Plastics Zellamid 250 GF 30 (PA6.6 + 30% glass fiber)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Zellamid® 250 GF 30 (PA 6.6 + 30% Glassfibre, black) is the registered trademark for Zell-Metall’s 30% glass fiber reinforced nylon grade 6.6. It offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining good wear resistance. It also allows higher max. service temperatures.

Fields: Transport and Conveyer Technology, Mechanical and Automotive Engineering, Precision Engineering, Processing Machinery.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/cc
Moisture Absorption at Equilibrium 1.5 %50% RH; ISO 1110; DIN 53714
Water Absorption at Saturation 5.5 %23°C; ISO 62; DIN 53495
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 175 MPaH 358/30; ISO 2039; DIN 53456
Tensile Strength at Break 160 MPaISO 527; DIN 53455
Elongation at Break 3.0 %ISO 527; DIN 53455
Tensile Modulus 11.0 GPaISO 527; DIN 53452
Charpy Impact, Notched 5.00 J/cm²double V-notch, rk=1.5 mm; DIN 53753
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 - 30.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Specific Heat Capacity 1.50 J/g-°CDIN 52612
Thermal Conductivity 0.270 W/m-KDIN 53612 Method A
Melting Point 255 °CISO 1218 Method A; DIN 53736
Maximum Service Temperature, Air 200 °Ca few hours operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75; DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75; DIN 53461
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
Quantum PEI - Ultem® 30% Glass Fiber Filled
Akro-Plastic Akromid® B3 GF 30 2 GIT (4618) PA 6 Dry, 30% Glass Filled
Akro-Plastic Akromid® A3 GF 30 1 black PA 6.6 Dry, 30% Glass Filled, Heat Stabilized
Covestro Makrolon® DP1-1888 Polycarbonate, 20% Glass Filled

PZELL04 / 72933

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.