MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® DP1-1888 Polycarbonate, 20% Glass Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes:
  • ISO 7391-PC,MR,(,,)-09-3,GF20
  • Developmental product
  • MVR (300 °C/1.2 kg) 10 cm3/10 min
  • 20 % Glass fiber reinforced
  • Milled fiber
  • Medium viscosity
  • Easy release
  • good surface quality
  • Injection molding - Melt temperature 310 - 330 °C
  • Available in intense black colors only
  • Precision parts in cameras

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Melt Density 1.14 g/cc
@Temperature 300 °C
0.0412 lb/in³
@Temperature 572 °F
Moisture Absorption at Equilibrium 0.10 %0.10 %Similar to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4,2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/inISO 294-4,2577
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
11 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527-1/-2
Elongation at Break 5.0 %5.0 %ISO 527-1/-2
Tensile Modulus 4.10 GPa595 ksiISO 527-1/-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Strength 36.0 kV/mm914 kV/inIEC 60243-1
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 55.0 µm/m-°C30.6 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°FMelt
Thermal Conductivity 0.211 W/m-K1.46 BTU-in/hr-ft²-°FMelt
Vicat Softening Point 144 °C291 °F50°C/h 50N; ISO 306
Flammability, UL94 V-2
@Thickness 2.00 mm
V-2
@Thickness 0.0787 in
IEC 60695-11-10
Oxygen Index 30 %30 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FInjection Molding; ISO 294
 310 - 330 °C590 - 626 °F
Mold Temperature 80.0 - 130 °C176 - 266 °F
 110 °C230 °FInjection Molding; ISO 10724
Ejection Temperature 140 °C284 °F
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 India
 Near East/Africa
 North America
 South and Central America
Eff. thermal diffusivity (m²/s)1.23E-07
FeatureRelease agent
FormPellets
ProcessInjection Molding
UL recognitionUL\lh\n

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® GF8001 Polycarbonate, 20% Glass Filled
Overview of materials for Polycarbonate, 20% Glass Filled
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced

PB09953 / 92793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.