MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Unifrax FyreWrap® Cable Insulation
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Unifrax's FyreWrap® Cable Insulation is a thin, flexible, insulation wrap designed to provide a fire-protective enclosure around cable trays and conduit. The FyreWrap system ensures electrical circuit integrity during exposure to an external hydrocarbon fire, permitting continued operation or controlled shutdown of critical equipment during emergency conditions. This system is FM Global approved and meets ASTM E-1725 "Fire Tests of Fire-Resistive Barrier Systems for Electrical System Components," the industry standard, requiring the highest level of performance for trays with zero to full cable loading. The system also meets ASTM E-1529 and provides circuit integrity ratings. FyreWrap complies with API and ExxonMobil specifications on fireproofing for petroleum and petrochemical processing plants.

    Product Components
  • Core Material: FyreWrap Cable Insulation products incorporate Insulfrax® Thermal Insulation as its core material. Insulfrax is a high-temperature insulation made from calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket form.
  • Encapsulating Material: The core insulation is completely encapsulated in an aluminum foil, fiberglass-reinforced scrim covering. This scrim provides additional handling strength as well as protection from tearing and moisture absorption. For outdoor installations, additional weather protection should be considered.
    • Typical System Properties
    • FM Global Approved - Wrap for Grouped Electrical Cables
    • API 2218 "Fireproofing Practices in Petroleum and Petrochemical Processing Plants" - complies
    • ExxonMobil GP14-03-01 "Fireproofing" Specification - complies
    • Fire Exposure - Hydrocarbon Fire per ASTM E-1529
    • Circuit Integrity - per ASTM E-1529
    • Temperature Integrity - per ASTM E-1725
    • Cable Loading - Empty to Fully Loaded Trays
    • Fire Rating - 30, 45, 60 minutes
    • ASTM E-84 Surface Burning Characteristics: (1) Unfaced Core: Flame/Smoke Rating = Zero, (2) FyreWrap: Flame/Smoke Rating < 25-50

    Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/ft³
Thickness 1500 mil
 2000 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound
Borealis Polycure™ PC531 Track Resistant Crosslinking Polyethylene Compound for Overhead Cable Insulation
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation
Chosun Refractories FRS 80 Flame-Gunning Repair Refractory
Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound

CUNIF111 / 97883

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.