MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Polycure™ PC531 Track Resistant Crosslinking Polyethylene Compound for Overhead Cable Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Polycure PC531 is a black, chemically crosslinking polyethylene compound that is designed for use in track resistant overhead cable insulation and jacketing.

Polycure PC531 is suitable for use in power cables rated up to 5kV. It also performs suitably in outdoor lighting cable applications such a airport and stadium lighting. PC531 is specifically suited for outdoor installations.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 17.69 MPa>= 2565 psiHeat Aging (7 days at 121°C); ASTM D412
 19.7 MPa2850 psiASTM D412
Elongation at Break 472.5 %472.5 %Heat Aging(7 days at 121°C); ASTM D412
 525 %525 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.82.8ASTM D150
Dielectric Strength >= 33.5 kV/mm>= 850 kV/inAt 40 mils; ASTM D149
Dissipation Factor 0.00400.0040ASTM D150
 
Processing PropertiesMetricEnglishComments
Front Barrel Temperature >= 118 °C>= 244 °F
Melt Temperature >= 124 °C>= 255 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis LE4217 Polyethylene Compound, Crosslinkable, Track Resistant
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation
Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound
Unifrax FyreWrap® Cable Insulation
Chevron Phillips HiD® 9402 HDPE Blow Molding Resin

PBOREA184 / 27491

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.