MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC GELOY™ XP7560 ASA (Europe)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA. Excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Water Absorption 0.80 %23°C/sat; ISO 62
Moisture Absorption 0.300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmSABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ISO 2039-2
Ball Indentation Hardness 92.0 MPaISO 2039-1
Tensile Strength at Break 43.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
Elongation at Break 20 %50 mm/min; ISO 527
Elongation at Yield 3.7 %50 mm/min; ISO 527
Tensile Modulus 2460 MPa1mm/min; ISO 527
Flexural Yield Strength 82.0 MPa2 mm/min; ISO 178
Flexural Modulus 2500 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
 95.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 102 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 102 °CRate B/50; ISO 306
 107 °CRate B/120; ISO 306
 113 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 230 - 260 °CInjection Molding
Zone 1 220 - 250 °C
Zone 2 230 - 260 °C
Zone 3 240 - 270 °C
Melt Temperature 250 - 270 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10159 / 243626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.