MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC GELOY™ XP7560 ASA (Europe)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA. Excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %23°C/sat; ISO 62
Moisture Absorption 0.300 %0.300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inSABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
20 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ISO 2039-2
Ball Indentation Hardness 92.0 MPa13300 psiISO 2039-1
Tensile Strength at Break 43.0 MPa6240 psi50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ISO 527
Elongation at Break 20 %20 %50 mm/min; ISO 527
Elongation at Yield 3.7 %3.7 %50 mm/min; ISO 527
Tensile Modulus 2.46 GPa357 ksi1mm/min; ISO 527
Flexural Yield Strength 82.0 MPa11900 psi2 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
52.8 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
 95.0 °C203 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 102 °C216 °FRate B/50; ISO 306
 107 °C225 °FRate B/120; ISO 306
 113 °C235 °FRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
UL 94 by SABIC-IP
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 230 - 260 °C446 - 500 °FInjection Molding
Zone 1 220 - 250 °C428 - 482 °F
Zone 2 230 - 260 °C446 - 500 °F
Zone 3 240 - 270 °C464 - 518 °F
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 90.0 - 100 °C194 - 212 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.050 %0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10159 / 243626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.