TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significant properties 1 hour after mixing. However, an extended cure of 4-6 hours at 25°C is required for fully matured bonds. Note: TRA-BOND 216R01 develops a high exotherm. Use immediately after mixing. The exothermic reaction begins within 2 minutes after initiating the mixing step, so have everything ready before removing the BIPAX clamp. Information provided by Tra-Con Inc. |