MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding and coil embedding applications where a desirable combination of superior mechanical and electrical properties plus fire retardancy and room temperature curing is required. This easy-to-use epoxy system has a low coefficient of thermal expansion, and exhibits excellent wetting and adhesion to most electronic and aerospace-industry materials (metals, glass products, ceramics, industrial laminates and many rigid plastics). Fully cured TRA-CAST 3143 is a durable electrical insulator, dimensionally stable over a wide temperature range, and is resistant to moisture, gases petroleum lubricants and fuels, salts, many mild acids and alkalis, and other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 400 cP
@Temperature 25.0 °C
400 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+14 ohm-cm5.00e+14 ohm-cm
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time 360 min6.00 hour4 hrs @ 25°C + 2 hrs @ 65°C
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 180 min180 min
 
Descriptive Properties
Color Black
Mix Ratio, parts by weight100/15Resin/Hardener
Thixotropic Index 1.25 rpm/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Cast 9182A Semi-Rigid Flame Retardant Epoxy Encapsulant
3M Jet-melt™ 3748 V-O Light Yellow Adhesive: High-Melt Technology
Dow SE 4445 CV KIT
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets
3M FM069 Indoor UL Recognized Brite Silver Polyester Label Products

PTRAC109 / 71037

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.