MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 985 Epoxy + Carbon Fabric Laminate
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 985 is a 350°F (177°C) curing epoxy resin system. CYCOM 985 is designed for use where a balance of performance and processing characteristics is required. It has excellent structural performance and good impact resistance. CYCOM 985 is co-curable with structural adhesives and will produce outstanding thin-skinned sandwich structures. CYCOM 985 allows thick section construction without exotherm problems. Optimum properties are achieved by curing under autoclave pressure from 45 to 100 psi (as appropriate to panel configuration) at 350°F (177°C) for two hours. CYCOM 985 prepregs have good tack and drape and an out-time of two weeks at room temperature.

Features & Benefits:

  • Modified epoxy system
  • Excellent hot/wet strength retention
  • 350°F (177°C) cure
  • Good impact resistance
  • 300°F (149°C) service temperature
  • Controlled flow
  • Ease of processing
  • Good tack and drape
  • 14 day shop life
  • Shelf life of 6 months at 0°F (-18°C)
Applications: Primary and secondary aircraft structures

Mechanical property data for 985 epoxy with 14 ply laminate with 57% fiber volume Carbon Fabric 3K70 PW

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 111000 psi
@Temperature 24.0 °C
90°, 20 ply
Tensile Modulus 57.0 GPa
@Temperature 177 °C
 59.0 GPa
@Temperature 132 °C
 59.0 GPa
@Temperature 24.0 °C
 60.0 GPa
@Temperature 71.0 °C
Compressive Strength 635 MPa
@Temperature -54.0 °C
 644 MPa
@Temperature 24.0 °C
Wet
 724 MPa
@Temperature 71.0 °C
 848 MPa
@Temperature 24.0 °C
Compressive Modulus 59000 MPa
@Temperature -54.0 °C
 59000 MPa
@Temperature 71.0 °C
 59000 MPa
@Temperature 132 °C
 61000 MPa
@Temperature 24.0 °C
Shear Strength 1000 psi
@Temperature 24.0 °C
Short Beam
 8100 psi
@Temperature 132 °C
Short Beam
 9000 psi
@Temperature 71.0 °C
Short Beam
 13900 psi
@Temperature -54.0 °C
Short Beam
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 149 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °F
@Time 7200 sec
Cure
Shelf Life 6.00 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 5320-1 Epoxy with T40/800B Unidirectional Tape Composite
Solvay CYCOM® 977-3 Epoxy - Unidirectional Carbon Fiber Tape
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with IM7-6K-4HS Fabric
Solvay CYCOM® 5250-4 RTM BMI Resin, Composite with T650-35-3K-PW Fabric
Solvay CYCOM® 890 RTM Resin - Woven Carbon Fabric Composite

PCYTED092c / 234741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.